| Availability: | |
|---|---|
| Quantity: | |
XRT-PLS
xinrui-te
550340
------XRT-MS
Made from 100% virgin polypropylene, Polypropylene mesh fiber resembles a fine net of interconnected monofilaments. When you mix it into concrete, the stirring and rubbing can break apart the horizontal connections, and the filaments or netting stretch out fully — so the concrete ends up being reinforced by a huge number of polypropylene fibers (over 7 million per m²).
Density (g/cm3) | 0.91+/-0.01 | Elastic Modulas (mPa) | > 4000 |
Equivalent Diameter (um) | 100 | Shape | Beam-like Net |
Crack Elongation(%) | ≥ 15 | Acid &Alkali Resistance | Strong |
Tensile Strength (MPa) | 400min. | Length (mm) | Times of 4mm or 6mm |
Melting Point (℃) | 160 –170 | Tensile Ratio (%) | 5-10 |
◆Inrease seepage resistance ◆Prolong endurance ◆Increase cracking resistance ◆Increase fire resistance ◆Strengthen spurt & fatigue
◆Improve tensile, bending & folding strength
◆Strong acid & alkali resistance and good endurance
◆Improve plastic deformity
Generally, the proper length of the fiber added to concrete is 18mm, and for spray concrete, it is 12mm.
Usually, the proper amount of concrete is 0.9kg/m3; the waterproof layer of the bridge requires 1.20-1.8kg/m3; the spray concrete in the tunnel is also 1.8kg/m3. The fiber has greater effects on concrete with active compound materials, such as silicon ash, coal powder, ground slag, and zeolite powder.
A double-axle horizontal mixer is preferable; a self-dropping cylinder mixer is also acceptable.
Crushed stones, fibers, and sand are fed into the mixer sequentially. After stirring for about 2-3 minutes, the fiber will fully spread. Then add cement and water, and stir again as per the normal process. The addition of materials can also be performed as usual, but the stirring time should be extended to more than 4 minutes to ensure the fiber is completely dispersed.
Here is s a quick, back‑of‑the‑envelope estimate—based on a few reasonable assumptions and typical U.S. labor‑rate ranges—of the approximate added labor cost per cubic meter / cubic yard when polypropylene mesh fibers are mixed into concrete.
Extra labor time (per m³ of concrete) | Lower-end hourly labor rate | Typical hourly labor rate |
$30/hr | $40/h | |
Negligible impact:0 min | 0 | 0 |
Low impact:5 min | $2.50/m³ | $3.33/m³ |
Moderate impact:10 min | $5.00/m³ | $6.67/m³ |
Noted:
1. If the fibers are just mixed in dry and the pumping/placement goes smoothly,
It’s usually “low impact” or “negligible.”
2.Quick formula: added cost ($/m³) = (hourly rate ÷ 60) × extra minutes.
Conclusion: In most cases, adding mesh fibers won’t raise labor costs — or only adds a tiny bit.
As a leading polypropylene mesh fiber factory, we specialize in producing premium virgin PP fibers for the global construction market. We offer high-quality polypropylene mesh fiber for sale in various lengths (such as 12mm and 18mm) to meet specific project requirements from tunnel shotcrete to bridge deck overlays. Whether you are looking for a trusted PP mesh fiber manufacturer or a wholesale concrete fiber supplier that provides competitive factory prices, XRT-MS is your ideal partner. Our advanced fibrillated design makes us a top-tier concrete reinforcement fiber supplier, delivering easy-to-disperse solutions that minimize labor impact while maximizing engineering performance.
Upgrade your concrete performance with our industry-leading XRT-MS mesh fibers. As a dedicated polypropylene fiber manufacturer, we offer comprehensive technical support, customized dosage recommendations, and competitive wholesale pricing for bulk international orders. Contact us now to receive our latest price list, technical data sheets, and a professional consultation to ensure your next project achieves the highest standards of stability and crack resistance
Learn how monofilament synthetic fibers provide 3D concrete reinforcement to prevent cracks, replace steel mesh, and enhance structural durability.
Optimize concrete floors with PP hybrid macro synthetic fibers. Replace steel mesh, stop cracks, and boost durability with dual-action reinforcement.
Learn to diagnose concrete mix imbalances. This guide covers water-cement ratios, admixture dosages, and testing to ensure structural durability.
Compare plasticizers vs. superplasticizers. Learn about water reduction, molecular mechanisms, and dosage to optimize concrete strength and budget.
Optimize industrial foam control with precise dosing, root cause analysis, and engineering strategies to prevent downtime and maximize process ROI.
Guide to steel fiber in concrete: Learn structural limits, ROI, and how to replace rebar in slabs and shotcrete for faster, more durable construction.
Learn how Polycarboxylate Superplasticizers (PCE) optimize concrete. Explore water reduction, UHPC/SCC applications, and expert selection strategies.
Master Polycarboxylate Superplasticizer (PCE) for high-strength concrete. Learn about its 50% water reduction, powder vs liquid, and applications.
Evaluate synthetic microfibers for construction and textiles. Balance structural performance with environmental compliance and sourcing risk mitigation.
Improve concrete workability and durability with sodium gluconate retarder. Learn about optimal dosage, chemical mechanisms, and project benefits.
Optimize concrete mix design with our guide to water-reducing agents. Evaluate PCE, SNF, and lignin to boost durability, strength, and workability.
Learn the difference between anti-foam agents and defoamers. Master preventive vs. reactive foam control to optimize industrial process efficiency.
Traditional concrete wall construction faces a long-standing set of operational challenges. Labor-intensive steel mesh installation consistently slows down project timelines. Over time, moisture penetration creates severe spalling risks as internal steel begins to corrode.
Traditional secondary reinforcement relies heavily on welded wire mesh. This approach demands significant manual labor. It frequently suffers from improper placement on job sites. Worse, it rarely prevents early-stage plastic shrinkage cracking.
Rising costs of heavily polymer-modified asphalt (PMA) and Stress Absorbing Membrane Interlayers (SAMI) are forcing pavement engineers to seek alternative mechanical reinforcement strategies.
Uncontrolled foam in industrial processes doesn't just look messy. It causes severe equipment cavitation and significantly reduces usable tank capacity. It also slows down production throughput and introduces critical defects into finished products.
Modern highway and industrial road construction faces massive pressure. Project owners demand aggressively accelerated timelines. They also expect extended lifecycle durability from every pavement slab.
Concrete contractors and specifying engineers face mounting operational challenges today. Unpredictable steel costs frequently squeeze tight project margins. Placing traditional welded wire mesh demands intensive manual labor and slows down pour schedules.
The concrete reinforcement industry is undergoing a massive shift. Engineers and contractors are rapidly moving away from labor-intensive traditional steel like rebar and wire mesh. Advanced engineered polymers now offer a smarter, highly efficient alternative for modern builds.
Managing foam generation remains a massive hurdle in food, beverage, and packaging production. Excess foam severely reduces processing throughput. It causes messy spillovers on facility floors. You must control this rapid macrofoam expansion without violating strict food-contact safety regulations.