| Availability: | |
|---|---|
| Quantity: | |
XRT-GFY
xinrui-te
-----– XRT-GFY
XRT-GFY glass fiber yarn is made from ultra-fine glass filaments, so it has high performance with strong tensile strength and good chemical resistance. That strong bonding and unique formula make the yarn a reliable, chemical-resistant glass-fiber yarn for concrete reinforcement, especially suited for thin-section concrete. As a high-strength glass fiber yarn manufacturer, we ensure precise sizing and filament control, so that using XRT-GFY adds strength and durability to concrete while providing a clean, refined finish.
1. Precast architectural panels, decorative concrete pieces, and custom
countertops.
2. Structural parts that need lightweight reinforcement without reducing
load capacity.
1. Auto parts (for example, body panels and structural reinforcements).
2. Marine uses- FRP boat hulls, offshore structures, and corrosion-resistant pipes.
3. Infrastructure-storage tanks, cooling towers, sanitary fixtures, and chemical-resistant ductwork.
| Test Item | Testing Standard | Specified Requirement | Test Result | Compliance Status |
|---|---|---|---|---|
| Roving Linear Density (TEX) | ISO 1889 | 2400 ± 120 TEX | 2426 TEX | PASS |
| Moisture Content (%) | ISO 3344 | ≤ 0.1% | 0.04% | PASS |
| Loss on Ignition (%) | ISO 3344 | 1.05 ± 0.10% | 1.06% | PASS |
| Stiffness (mm) | ISO 3375 | 120 ± 20 mm | 134 mm | PASS |
| Beam Ratic (%) | Proprietary Method | > 85% | 91.12% | PASS |
*Note: "Beam Ratic" corrected to Beam Tenacity (assumed typo; if "Ratic" is a proprietary term, retain as-is with clarification).
Reference Standards:
International: ISO 1889, ISO 3344, ISO 3375
National: GB/T 18369–2001 (Chinese Standard for Glass Fiber Rovings)
Test Conditions:
Ambient Temperature: 20°C (±2°C)
Relative Humidity: 70% (±5%)
1. High tensile modulus helps reinforce concrete and cut down on cracks when it bends.
2. Low stretch at break keeps things dimensionally stable under heavy loads.
1. Resists alkalis in concrete and harsh industrial chemicals.
2. Marine-grade corrosion resistance for offshore and coastal structures.
1. Spray-friendly design lets fibers spread evenly and line up consistently.
2. Sizing improves resin wetting, reduces voids, and makes composites stronger.
1. Thoroughly tested to meet national and international standards for reliability and traceability.
2. Consistent batches ensure the same results in large-scale production.
While optimized for concrete reinforcement, XRT-GFY's versatility extends to:
Aerospace: Lightweight composite components for non-structural applications.
Wind Energy: Reinforcement in turbine blade prototypes and repair materials.
Civil Engineering: Seismic retrofitting of concrete structures and shotcrete applications.
1. Q: Is XRT-GFY glass fiber yarn suitable for thin-wall concrete and GRC sculpture?
A: Absolutely. Our ultra-fine glass filament yarn features high tensile strength and soft texture, which won’t block the mold surface
during casting. The glass fiber yarn delivers delicate surface finish for thin-section concrete, GRC wall cladding and concrete
sculptures without visible fiber marks.
2. Q: How much XRT-GFY glass fiber yarn should be added into concrete mortar?
A: Standard dosage of this glass fiber yarn for concrete reinforcement is 1.2%–2.5% by cement weight. For ultra-thin concrete
components or anti-crack mortar, we suggest 2.0%–3.0% dosage. Free mixing proportion test samples are available for bulk
buyers to adjust formula.
3. Q: Will glass fiber yarn cause pumping blockage during concrete construction?
A: Our XRT-GFY glass fiber yarn adopts precise filament control and a special sizing formula; filaments disperse independently in
With a proper mixing process, the fiberglass yarn has great pumpability and will not cause pipeline blockage in
commercial concrete production lines.
4. Q: Can you customize the specifications of glass fiber yarn for concrete reinforcement?
A: As professional high-strength glass fiber yarn manufacturer, we support customized filament thickness, yarn tex, sizing formula
and package for concrete anti-crack projects. We adjust custom sizing to match customer’s cement, polycarboxylate
superplasticizer and concrete additives system.
5. Q: What advantages does custom sizing glass fiber yarn bring to concrete mixing?
A: Custom sizing treatment is the core technology of our glass fiber yarn for concrete reinforcement. It strengthens bonding force
between glass filaments and cement matrix, realizes uniform fiber dispersion during mixing, avoids fiber agglomeration, lowers
water demand of concrete mix, and ensures consistent anti-crack performance for thin-section concrete.
Learn how monofilament synthetic fibers provide 3D concrete reinforcement to prevent cracks, replace steel mesh, and enhance structural durability.
Improve concrete workability and durability with sodium gluconate retarder. Learn about optimal dosage, chemical mechanisms, and project benefits.
Optimize concrete floors with PP hybrid macro synthetic fibers. Replace steel mesh, stop cracks, and boost durability with dual-action reinforcement.
Learn to diagnose concrete mix imbalances. This guide covers water-cement ratios, admixture dosages, and testing to ensure structural durability.
Compare plasticizers vs. superplasticizers. Learn about water reduction, molecular mechanisms, and dosage to optimize concrete strength and budget.
Optimize industrial foam control with precise dosing, root cause analysis, and engineering strategies to prevent downtime and maximize process ROI.
Guide to steel fiber in concrete: Learn structural limits, ROI, and how to replace rebar in slabs and shotcrete for faster, more durable construction.
Learn how Polycarboxylate Superplasticizers (PCE) optimize concrete. Explore water reduction, UHPC/SCC applications, and expert selection strategies.
Master Polycarboxylate Superplasticizer (PCE) for high-strength concrete. Learn about its 50% water reduction, powder vs liquid, and applications.
Evaluate synthetic microfibers for construction and textiles. Balance structural performance with environmental compliance and sourcing risk mitigation.
Optimize concrete mix design with our guide to water-reducing agents. Evaluate PCE, SNF, and lignin to boost durability, strength, and workability.
Learn the difference between anti-foam agents and defoamers. Master preventive vs. reactive foam control to optimize industrial process efficiency.
Traditional concrete wall construction faces a long-standing set of operational challenges. Labor-intensive steel mesh installation consistently slows down project timelines. Over time, moisture penetration creates severe spalling risks as internal steel begins to corrode.
Traditional secondary reinforcement relies heavily on welded wire mesh. This approach demands significant manual labor. It frequently suffers from improper placement on job sites. Worse, it rarely prevents early-stage plastic shrinkage cracking.
Rising costs of heavily polymer-modified asphalt (PMA) and Stress Absorbing Membrane Interlayers (SAMI) are forcing pavement engineers to seek alternative mechanical reinforcement strategies.
Uncontrolled foam in industrial processes doesn't just look messy. It causes severe equipment cavitation and significantly reduces usable tank capacity. It also slows down production throughput and introduces critical defects into finished products.
Modern highway and industrial road construction faces massive pressure. Project owners demand aggressively accelerated timelines. They also expect extended lifecycle durability from every pavement slab.
Concrete contractors and specifying engineers face mounting operational challenges today. Unpredictable steel costs frequently squeeze tight project margins. Placing traditional welded wire mesh demands intensive manual labor and slows down pour schedules.
The concrete reinforcement industry is undergoing a massive shift. Engineers and contractors are rapidly moving away from labor-intensive traditional steel like rebar and wire mesh. Advanced engineered polymers now offer a smarter, highly efficient alternative for modern builds.
Managing foam generation remains a massive hurdle in food, beverage, and packaging production. Excess foam severely reduces processing throughput. It causes messy spillovers on facility floors. You must control this rapid macrofoam expansion without violating strict food-contact safety regulations.